ASME SA 387 GRADE 11 Class 2

Our alloy steel SA 387 GR. 5 CL. 1/2 plates are expertly crafted for deployment in steel pressure vessels operating at high temperatures and challenging environments. The core composition of this alloy steel incorporates molybdenum, imparting remarkable tensile strength and impressive resistance to corrosion. These plates adhere strictly to the guidelines of ASME SA387, an industry-standard specification governing the production of welded molybdenum steel plates. Their prominence is especially notable in applications requiring performance in elevated temperature conditions.
SA387/ASME SA 387 GRADE 9 Class 2 Class 2Plate Specification
Specifications |
: |
ASTM A387 / ASME SA387 |
Thickness |
: |
5mm-150mm |
Width |
: |
1000mm-4500mm |
Length |
: |
3000mm -18000mm |
Hardness |
: |
As per ASME A & NACE MR 175 |
Impact Tested |
: |
Impact tested -52° C |
Finish |
: |
Hot rolled plate (HR), Cold rolled sheet (CR) |
Chemical Requirements
Element |
|
Chemical Composition (%) |
|
|
SA 387 Grade 5 |
Carbon: |
Heat Analysis: |
0.15 max |
|
Product Analysis: |
0.15 max |
Manganese: |
Heat Analysis: |
0.30 - 0.60 |
|
Product Analysis: |
0.25 - 0.66 |
Phosphorus: |
Heat Analysis: |
0.035 |
|
Product Analysis: |
0.035 |
Sulphur (max): |
Heat Analysis: |
0.030 |
|
Product Analysis: |
0.030 |
Silicon: |
Heat Analysis: |
0.50 max |
|
Product Analysis: |
0.55 max |
Chromium: |
Heat Analysis: |
4.00 - 6.00 |
|
Product Analysis: |
3.90 - 6.10 |
Molybdenum: |
Heat Analysis: |
0.45 - 0.65 |
|
Product Analysis: |
0.40 - 0.70 |
The carbon content for plates over 5 in. (125 mm) in thickness is 0.17 max on product
analysis.
Mechanical Composition
Tensile Strength |
Yield Strength |
Elongation in 50mm (%) |
Reduction of area in % |
75-100 ksi, 515-690 MPa |
45 Ksi, 310 MPa |
18 |
45 |